Best quality Cw110c Threadlet - C19160 alloy – Kinkou
Best quality Cw110c Threadlet - C19160 alloy – Kinkou Detail:
1. Physical properties of C19160
Density | 8.86g/cm3 |
Thermal expansion coefficient | 17.7×10^-6/k |
Thermal conductivity | 210W/(m·K) |
Conductivity | >50%IACS |
Elastic Modulus |
120GPa |
2. Mechanical properties of C19160
State |
size |
Tensile strength |
Yield strength |
Elongation |
Conductivity |
Hardness |
MPa |
MPa |
% |
%ICAS |
HV0.2 |
||
TB00 |
≤40 |
220-360 |
46-72 |
38-45 |
30 |
- |
TH |
≤10 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
10-30 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
|
30-40 |
440-470 |
220-350 |
20-27 |
51-61 |
- |
|
TL |
≤5.0 |
≥620 |
- |
≥5 |
≥50 |
≥165 |
5-6 |
≥590 |
- |
≥5 |
≥50 |
≥165 |
|
6-9.5 |
≥570 |
- |
≥5 |
≥50 |
≥165 |
|
≥9.5 |
≥550 |
- |
≥5 |
≥50 |
≥165 |
3. Application of C19160
C19160 is mainly used in pins, sockets and conductive spring contacts with high strength and elasticity.
Product detail pictures:
Related Product Guide:
Being supported by an highly developed and skilled IT group, we could offer you technical support on pre-sales & after-sales support for Best quality Cw110c Threadlet - C19160 alloy – Kinkou , The product will supply to all over the world, such as: Korea, Portugal, Salt Lake City, Honest to every customers are our requested! First-class serve, best quality, best price and fastest delivery date is our advantage! Give every customers good serve is our tenet! This makes our company get the favour of customers and support! Welcome all over the world customers send us enquiry and looking forward your good co-operation !Make sure you your inquiry for more details or request for dealership in selected regions.
By Karl from Florida - 2017.06.16 18:23
Speaking of this cooperation with the Chinese manufacturer, I just want to say"well dodne", we are very satisfied.
By Ivy from Malaysia - 2018.12.05 13:53
Write your message here and send it to us