1. Physical properties of C19160
Density | 8.86g/cm3 |
Thermal expansion coefficient | 17.7×10^-6/k |
Thermal conductivity | 210W/(m·K) |
Conductivity | >50%IACS |
Elastic Modulus |
120GPa |
2. Mechanical properties of C19160
State |
size |
Tensile strength |
Yield strength |
Elongation |
Conductivity |
Hardness |
MPa |
MPa |
% |
%ICAS |
HV0.2 |
||
TB00 |
≤40 |
220-360 |
46-72 |
38-45 |
30 |
- |
TH |
≤10 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
10-30 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
|
30-40 |
440-470 |
220-350 |
20-27 |
51-61 |
- |
|
TL |
≤5.0 |
≥620 |
- |
≥5 |
≥50 |
≥165 |
5-6 |
≥590 |
- |
≥5 |
≥50 |
≥165 |
|
6-9.5 |
≥570 |
- |
≥5 |
≥50 |
≥165 |
|
≥9.5 |
≥550 |
- |
≥5 |
≥50 |
≥165 |
3. Application of C19160
C19160 is mainly used in pins, sockets and conductive spring contacts with high strength and elasticity.
Product detail pictures:
Related Product Guide:
We have been commitment to supply the competitive price ,excellent products and solutions high-quality, at the same time as fast delivery for Best quality Cw110c Threadlet - C19160 alloy – Kinkou , The product will supply to all over the world, such as: US, Melbourne, Istanbul, Our products have won an excellent reputation at each of the related nations. Because the establishment of our firm. we have insisted on our production procedure innovation together with the most recent modern day managing method, attracting a sizable quantity of talents within this industry. We regard the solution good quality as our most vital essence character.
By Nicola from Colombia - 2017.06.16 18:23
It's really lucky to find such a professional and responsible manufacturer, the product quality is good and delivery is timely, very nice.
By Clementine from Jakarta - 2018.07.27 12:26
Write your message here and send it to us