Copper Nickel Cobalt Beryllium Alloy Rod And Wire(CuNiBe C17510)
1. Chemical Composition of C17510
Model |
Be |
Co |
Ni |
Fe |
Al |
Si |
Cu |
C17510 |
0.2-0.6 |
≤0.3 |
1.4-2.2 |
≤0.1 |
≤0.20 |
≤0.20 |
Remnant |
2. Physical And Mechanical Properties of C17510
State |
Performance |
|||
Standard Code |
Category |
Tensile Strength(MPa) |
Hardness(HRB) |
Electrical Conductivity(IACS,%) |
TB00 |
Solid Solution Treatment(A) |
240-380 |
Min50 |
20 |
TD04 |
Solid Solution Treatment & Cold Process Hardening State(H) |
450-550 |
60-80 |
20 |
|
After Heat Treatment Of Deposit |
|||
TF00 |
Heat Treatment Of Deposit(AT) |
690-895 |
92-100 |
45 |
TH04 |
Hardening & Deposit Heat Treatment of Settlement(HT) |
760-965 |
95-102 |
48 |
3. Application Fields of C17510
It is mainly used for welding,new-energy automobile charging pile and communication industry