Europe style for Cuni1co1be Rod - C19160 alloy – Kinkou
Europe style for Cuni1co1be Rod - C19160 alloy – Kinkou Detail:
1. Physical properties of C19160
Density | 8.86g/cm3 |
Thermal expansion coefficient | 17.7×10^-6/k |
Thermal conductivity | 210W/(m·K) |
Conductivity | >50%IACS |
Elastic Modulus |
120GPa |
2. Mechanical properties of C19160
State |
size |
Tensile strength |
Yield strength |
Elongation |
Conductivity |
Hardness |
MPa |
MPa |
% |
%ICAS |
HV0.2 |
||
TB00 |
≤40 |
220-360 |
46-72 |
38-45 |
30 |
- |
TH |
≤10 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
10-30 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
|
30-40 |
440-470 |
220-350 |
20-27 |
51-61 |
- |
|
TL |
≤5.0 |
≥620 |
- |
≥5 |
≥50 |
≥165 |
5-6 |
≥590 |
- |
≥5 |
≥50 |
≥165 |
|
6-9.5 |
≥570 |
- |
≥5 |
≥50 |
≥165 |
|
≥9.5 |
≥550 |
- |
≥5 |
≥50 |
≥165 |
3. Application of C19160
C19160 is mainly used in pins, sockets and conductive spring contacts with high strength and elasticity.
Product detail pictures:
Related Product Guide:
In order to best meet client's needs, all of our operations are strictly performed in line with our motto "High Quality, Competitive Price, Fast Service" for Europe style for Cuni1co1be Rod - C19160 alloy – Kinkou , The product will supply to all over the world, such as: Pakistan, Honduras, kazakhstan, We always adhere to follow the honesty, mutual benefit, common development, after years of development and the tireless efforts of all staff, now has perfect export system, diversified logistics solutions, thorough meet customer shipping, air transport, international express and logistics services. Elaborate one-stop sourcing platform for our customers!
By Pandora from Slovenia - 2018.12.11 14:13
The factory technical staff gave us a lot of good advice in the cooperation process, this is very good, we are very grateful.
By Maureen from Haiti - 2017.11.20 15:58
Write your message here and send it to us