SUZHOU KINKOU E-TECH CO.,LTD.
jinjiang@kinkou.cn
+8613773014250
English
Home
About Us
Company Profile
Products
Feature products
C17200
C17300
C17500
C17510
C18150
C72900
KINKOU T-250/45
QA
Certificate
Testing Equipment
R & D
R & D
Patent
Application
Chemical Industry
5G
Oil & Gas & Mining Industry
Automotive
Others
News
Contact
Home
Featured
Best Price on Cw106c Bar - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou
1. Chemical Composition of CuCrZr Alloy Micro Bore Precision Tube Model Ni Fe Pb Sn Zr Cu C15100 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.15-0.30 Remnant C15200 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.30-0.50 Remnant Model Cr Fe Pb Si Zr Cu C18150 0.5-1.5 - - - 0.05-0.25 Remnant C18200 0.6-1.2 ≤0.10 ≤0.05 ≤0.01 - Remnant 2. High Precision Indicator(TH04) of CuCrZr Alloy Micro Bore Precision Tube Item External Diameter ...
inquiry
detail
New Fashion Design for Cw110c Bar - Copper Cobalt Beryllium Alloy Rod And Wire(CuCoBe C17500) – Kinkou
1. Chemical Composition of C17500 Model Be Co Ni Fe Al Si Cu C17500 0.4-0.7 2.4-2.7 - ≤0.1 ≤0.20 ≤0.20 Remnant 2. Physical And Mechanical Properties of C17500 State Performance Standard Code Category Tensile Strength(MPa) Hardness(HRB) Electrical Conductivity(IACS,%) TB00 Solid Solution Treatment(A) 240-380 Min50 20 TD04 Solid Solution Treatment & Cold Process Hardening State(H) 450-550 60-80 20 Aft...
inquiry
detail
High reputation C17300 Foil - C19160 alloy – Kinkou
1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
inquiry
detail
Factory For C18200 Strip - KINKOU-96 copper alloy(Cu-9Ni-6Sn C72700) – Kinkou
1. Chemical Composition of C72700 Model Ni Sn Mn Pb Zn Fe P Impurities Cu C72700 8.5-9.5 5.5-6.5 0.05-0.3 ≤0.03 ≤0.15 ≤0.05 ≤0.05 ≤0.5 Remnant 2. Physical Properties of C72700 Density 8.9 (g/cm3) Melting Point 968-1078 (℃) Thermal Expansion Coefficient 17.25 (X10-6/℃) 20-200℃ Elastic Modulus 120 (GPa) Electrical Resistivity at 20℃ μΩ*cm Quench ≤19.5 Precipitation Hardening ≤15 Ele...
inquiry
detail
Best quality Cw110c Threadlet - C19160 alloy – Kinkou
1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
inquiry
detail
Reasonable price Cw106c Tube - KINKOU158 copper alloy(Cu-Ni-Sn C72900) – Kinkou
* Achieve a combination of high rigidity and high strength. Can withstand dynamic impact loads. Can meet the most stringent requirements of static structural load and pressure. The thermal stress relaxation resistance is significantly better than beryllium copper alloy. 2. Excellent performance of anti-wear bearing, with the valuable performance of natural self-lubrication without friction pair seizure, it is a necessary material for the landing gear bearing of large aircraft, and is also the...
inquiry
detail
Cheap price C17200 Foil - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou
1. Chemical Composition of CuCrZr Alloy Micro Bore Precision Tube Model Ni Fe Pb Sn Zr Cu C15100 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.15-0.30 Remnant C15200 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.30-0.50 Remnant Model Cr Fe Pb Si Zr Cu C18150 0.5-1.5 - - - 0.05-0.25 Remnant C18200 0.6-1.2 ≤0.10 ≤0.05 ≤0.01 - Remnant 2. High Precision Indicator(TH04) of CuCrZr Alloy Micro Bore Precision Tube Item External Diameter ...
inquiry
detail
High definition Cuni2be Foil - C19160 alloy – Kinkou
1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
inquiry
detail
Ordinary Discount Cucrzr Strip - C19160 alloy – Kinkou
1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
inquiry
detail
Manufacturing Companies for C15200 Bar - Al2O3 Dispersion Strengthened Copper Rod And Wire(C15715,C15725,C15760) – Kinkou
*The dispersion strengthened copper alloy has excellent resistance to high temperature softening in addition to good electrical ad thermal conductivity.It is one of the best among all high-conductivity and high-temperature copper alloys. *Our high-strength and high-conductivity Al2O3 dispersion strengthened copper wire rods take the place of imported equivalents due to high performance indexes.A roll of finished product weighs 150kg *It was assessed as Jiangsu high-tech product(for new materi...
inquiry
detail
China Gold Supplier for Cu15ni8sn Strip - Silicon Bronze Alloy(QSi1-3) – Kinkou
1. Chemical Composition of QSi1-3 Model Si Fe Ni Zn Pb Mn Sn Al Cu QSi1-3 0.6-1.10 0.1 2.4-3.4 0.2 0.15 0.1-0.4 0.1 0.02 Remnant 2. Physical Properties of QSi1-3 Model Tensile Strength Elongation Hardness MPa % HBS QSi1-3 >490 >10% 170-240 3. Application of QSi1-3 QSi1-3 is used to manufacture friction parts (such as engine exhaust and intake valve guide sleeves) and structural parts that work in corrosive media...
inquiry
detail
Top Suppliers C17200 Bar - Copper ferro alloy – Kinkou
Copper ferro alloy has the same electrical conductivity, thermal conductivity, ductility, elasticity and other wear resistance, tensile strength, hardness, and magnetic properties as iron. The alloy ratio of copper and iron can be freely adjusted as needed. The ratio of copper can be from 10% to 90%. 1. Application of copper ferro alloy Copper ferro alloy is mainly used in RF shielding net,connectors,mold and so on. 2. Products of Copper Ferro Alloy Copper ferro alloy rod,copper ferro alloy w...