• Factory best selling Cuni2be Threadlet - C19160 alloy – Kinkou

    Factory best selling Cuni2be Threadlet - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • Cheapest Price Cw104c Bar - Copper ferro alloy – Kinkou

    Cheapest Price Cw104c Bar - Copper ferro alloy – Kinkou

    Copper ferro alloy has the same electrical conductivity, thermal conductivity, ductility, elasticity and other wear resistance, tensile strength, hardness, and magnetic properties as iron. The alloy ratio of copper and iron can be freely adjusted as needed. The ratio of copper can be from 10% to 90%. 1. Application of copper ferro alloy Copper ferro alloy is mainly used in RF shielding net,connectors,mold and so on. 2. Products of Copper Ferro Alloy Copper ferro alloy rod,copper ferro alloy w...
  • factory Outlets for C15715 Rod - Copper ferro alloy – Kinkou

    factory Outlets for C15715 Rod - Copper ferro alloy – Kinkou

    Copper ferro alloy has the same electrical conductivity, thermal conductivity, ductility, elasticity and other wear resistance, tensile strength, hardness, and magnetic properties as iron. The alloy ratio of copper and iron can be freely adjusted as needed. The ratio of copper can be from 10% to 90%. 1. Application of copper ferro alloy Copper ferro alloy is mainly used in RF shielding net,connectors,mold and so on. 2. Products of Copper Ferro Alloy Copper ferro alloy rod,copper ferro alloy w...
  • 100% Original Copper Nickel Tube - KINKOU158 copper alloy(Cu-Ni-Sn C72900) – Kinkou

    100% Original Copper Nickel Tube - KINKOU158 copper alloy(Cu-Ni-Sn C72900) – Kinkou

    * Achieve a combination of high rigidity and high strength. Can withstand dynamic impact loads. Can meet the most stringent requirements of static structural load and pressure. The thermal stress relaxation resistance is significantly better than beryllium copper alloy. 2. Excellent performance of anti-wear bearing, with the valuable performance of natural self-lubrication without friction pair seizure, it is a necessary material for the landing gear bearing of large aircraft, and is also the...
  • Best quality C18200 Wire - KINKOU-High Precision Beryllium Copper Wire(C17200) – Kinkou

    Best quality C18200 Wire - KINKOU-High Precision Beryllium Copper Wire(C17200) – Kinkou

    1. Chemical Composition of KINKOU-High Precision Beryllium Copper Wire Model Be Ni+Co Ni+Co+Fe Ni+Co+Fe+Be+Cu C17200 1.8-2.0 ≥0.20 ≤0.6 ≥99.5 2. Physical Properties of KINKOU-High Precision Beryllium Copper Wire Diameter Tensile Strength(MPa) ≤φ0.20mm 784-1078 >φ0.20mm 686-980 3. Dimension and Allowable Deviation of KINKOU-High Precision Beryllium Copper Wire Size φ0.03-φ0.09 φ0.10-φ0.29 φ0.30-φ1.0 Allowable Deviation -0.003 ...
  • Hot sale Cw104c Tube - C19160 alloy – Kinkou

    Hot sale Cw104c Tube - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • Wholesale Cw103c Tube - Silicon Bronze Alloy(QSi1-3) – Kinkou

    Wholesale Cw103c Tube - Silicon Bronze Alloy(QSi1-3) – Kinkou

    1. Chemical Composition of QSi1-3 Model Si Fe Ni Zn Pb Mn Sn Al Cu QSi1-3 0.6-1.10 0.1 2.4-3.4 0.2 0.15 0.1-0.4 0.1 0.02 Remnant 2. Physical Properties of QSi1-3 Model Tensile Strength Elongation Hardness MPa % HBS QSi1-3 >490 >10% 170-240 3. Application of QSi1-3 QSi1-3 is used to manufacture friction parts (such as engine exhaust and intake valve guide sleeves) and structural parts that work in corrosive media...
  • Factory Price For Cube Bar - KINKOU-96 copper alloy(Cu-9Ni-6Sn  C72700) – Kinkou

    Factory Price For Cube Bar - KINKOU-96 copper alloy(Cu-9Ni-6Sn C72700) – Kinkou

    1. Chemical Composition of C72700 Model Ni Sn Mn Pb Zn Fe P Impurities Cu C72700 8.5-9.5 5.5-6.5 0.05-0.3 ≤0.03 ≤0.15 ≤0.05 ≤0.05 ≤0.5 Remnant 2. Physical Properties of C72700 Density 8.9 (g/cm3) Melting Point 968-1078 (℃) Thermal Expansion Coefficient 17.25 (X10-6/℃) 20-200℃ Elastic Modulus 120 (GPa) Electrical Resistivity at 20℃   μΩ*cm Quench ≤19.5   Precipitation Hardening ≤15   Ele...
  • Hot sale C15725 Threadlet - Copper Cobalt Beryllium Alloy Rod And Wire(CuCoBe C17500) – Kinkou

    Hot sale C15725 Threadlet - Copper Cobalt Beryllium Alloy Rod And Wire(CuCoBe C17500) – Kinkou

    1. Chemical Composition of C17500 Model Be Co Ni Fe Al Si Cu C17500 0.4-0.7 2.4-2.7 - ≤0.1 ≤0.20 ≤0.20 Remnant 2. Physical And Mechanical Properties of C17500 State Performance Standard Code Category Tensile Strength(MPa) Hardness(HRB) Electrical Conductivity(IACS,%) TB00 Solid Solution Treatment(A) 240-380 Min50 20 TD04 Solid Solution Treatment & Cold Process Hardening State(H) 450-550 60-80 20   Aft...
  • 8 Year Exporter C15100 Bar - C19160 alloy – Kinkou

    8 Year Exporter C15100 Bar - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • High definition C15730 Tube - KINKOU-96 copper alloy(Cu-9Ni-6Sn  C72700) – Kinkou

    High definition C15730 Tube - KINKOU-96 copper alloy(Cu-9Ni-6Sn C72700) – Kinkou

    1. Chemical Composition of C72700 Model Ni Sn Mn Pb Zn Fe P Impurities Cu C72700 8.5-9.5 5.5-6.5 0.05-0.3 ≤0.03 ≤0.15 ≤0.05 ≤0.05 ≤0.5 Remnant 2. Physical Properties of C72700 Density 8.9 (g/cm3) Melting Point 968-1078 (℃) Thermal Expansion Coefficient 17.25 (X10-6/℃) 20-200℃ Elastic Modulus 120 (GPa) Electrical Resistivity at 20℃   μΩ*cm Quench ≤19.5   Precipitation Hardening ≤15   Ele...
  • Best-Selling C15730 Rod - Copper Nickel Cobalt Beryllium Alloy Rod And Wire(CuNiBe C17510) – Kinkou

    Best-Selling C15730 Rod - Copper Nickel Cobalt Beryllium Alloy Rod And Wire(CuNiBe C17510) – Kinkou

    1. Chemical Composition of C17510 Model Be Co Ni Fe Al Si Cu C17510 0.2-0.6 ≤0.3 1.4-2.2 ≤0.1 ≤0.20 ≤0.20 Remnant 2. Physical And Mechanical Properties of C17510 State Performance Standard Code Category Tensile Strength(MPa) Hardness(HRB) Electrical Conductivity(IACS,%) TB00 Solid Solution Treatment(A) 240-380 Min50 20 TD04 Solid Solution Treatment & Cold Process Hardening State(H) 450-550 60-80 20   ...