• Chinese Professional C17200 Tube - C19160 alloy – Kinkou

    Chinese Professional C17200 Tube - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • High Quality for C72700 Foil - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    High Quality for C72700 Foil - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    1. Chemical Composition of CuCrZr Alloy Micro Bore Precision Tube Model Ni Fe Pb Sn Zr Cu C15100 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.15-0.30 Remnant C15200 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.30-0.50 Remnant Model Cr Fe Pb Si Zr Cu C18150 0.5-1.5 - - - 0.05-0.25 Remnant C18200 0.6-1.2 ≤0.10 ≤0.05 ≤0.01 - Remnant 2. High Precision Indicator(TH04) of CuCrZr Alloy Micro Bore Precision Tube Item External Diameter ...
  • Professional China Cuni2be - High Precision Beryllium Copper Tube C17200 – Kinkou

    Professional China Cuni2be - High Precision Beryllium Copper Tube C17200 – Kinkou

    Developed high-precision beryllium copper seamless pipe for 5G base station. At present, it is the only domestic manufacturer of high-quality beryllium copper seamless pipe with stable quality and mass supply. The outer diameter can be 1.0 ~ 25mm and the wall thickness is 0.08 ~ 6mm , The tolerance can be accurate to ± 0.01mm. The company’s regular supply of 2.0 * 1.6 2.0 * 1.8 3.5 * 3.2 3.95 * 3.65 and other high-precision beryllium copper seamless pipes have been widely used in 5G bas...
  • Hot sale Cw104c Tube - C19160 alloy – Kinkou

    Hot sale Cw104c Tube - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • Reasonable price Cw106c Tube - KINKOU-96 copper alloy(Cu-9Ni-6Sn  C72700) – Kinkou

    Reasonable price Cw106c Tube - KINKOU-96 copper alloy(Cu-9Ni-6Sn C72700) – Kinkou

    1. Chemical Composition of C72700 Model Ni Sn Mn Pb Zn Fe P Impurities Cu C72700 8.5-9.5 5.5-6.5 0.05-0.3 ≤0.03 ≤0.15 ≤0.05 ≤0.05 ≤0.5 Remnant 2. Physical Properties of C72700 Density 8.9 (g/cm3) Melting Point 968-1078 (℃) Thermal Expansion Coefficient 17.25 (X10-6/℃) 20-200℃ Elastic Modulus 120 (GPa) Electrical Resistivity at 20℃   μΩ*cm Quench ≤19.5   Precipitation Hardening ≤15   Ele...
  • OEM Customized C15715 Foil - C19160 alloy – Kinkou

    OEM Customized C15715 Foil - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • Short Lead Time for C17200 Rod - C19160 alloy – Kinkou

    Short Lead Time for C17200 Rod - C19160 alloy – Kinkou

    1. Physical properties of C19160 Density 8.86g/cm3 Thermal expansion coefficient 17.7×10^-6/k Thermal conductivity 210W/(m·K) Conductivity >50%IACS Elastic Modulus 120GPa 2. Mechanical properties of C19160 State size Tensile strength Yield strength Elongation Conductivity Hardness MPa MPa % %ICAS HV0.2 TB00 ≤40 220-360 46-72 38-45 30 - TH ≤10 490-550 410-490 15-20 60-51 - 10-30 490-550 410-490 15-20...
  • Bottom price Beryllium Copper Bar - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    Bottom price Beryllium Copper Bar - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    1. Chemical Composition of CuCrZr Alloy Micro Bore Precision Tube Model Ni Fe Pb Sn Zr Cu C15100 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.15-0.30 Remnant C15200 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.30-0.50 Remnant Model Cr Fe Pb Si Zr Cu C18150 0.5-1.5 - - - 0.05-0.25 Remnant C18200 0.6-1.2 ≤0.10 ≤0.05 ≤0.01 - Remnant 2. High Precision Indicator(TH04) of CuCrZr Alloy Micro Bore Precision Tube Item External Diameter ...
  • OEM/ODM Manufacturer Cw101c Foil - Copper Cobalt Beryllium Alloy Rod And Wire(CuCoBe C17500) – Kinkou

    OEM/ODM Manufacturer Cw101c Foil - Copper Cobalt Beryllium Alloy Rod And Wire(CuCoBe C17500) – Kinkou

    1. Chemical Composition of C17500 Model Be Co Ni Fe Al Si Cu C17500 0.4-0.7 2.4-2.7 - ≤0.1 ≤0.20 ≤0.20 Remnant 2. Physical And Mechanical Properties of C17500 State Performance Standard Code Category Tensile Strength(MPa) Hardness(HRB) Electrical Conductivity(IACS,%) TB00 Solid Solution Treatment(A) 240-380 Min50 20 TD04 Solid Solution Treatment & Cold Process Hardening State(H) 450-550 60-80 20   Aft...
  • 2020 Latest Design Cube Rod - Free Cutting Beryllium Copper Rod C15760 – Kinkou

    2020 Latest Design Cube Rod - Free Cutting Beryllium Copper Rod C15760 – Kinkou

    Free Cutting Beryllium Copper Rod C15760, C15760, *The dispersion strengthened copper alloy has excellent resistance to high temperature softening in addition to good electrical ad thermal conductivity.It is one of the best among all high-conductivity and high-temperature copper alloys. *Our high-strength and high-conductivity Al2O3 dispersion strengthened copper wire rods take the place of imported equivalents due to high performance indexes.A roll of finished product weighs 150kg *It was ...
  • Fast delivery Cucrzr Foil - Copper ferro alloy – Kinkou

    Fast delivery Cucrzr Foil - Copper ferro alloy – Kinkou

    Copper ferro alloy has the same electrical conductivity, thermal conductivity, ductility, elasticity and other wear resistance, tensile strength, hardness, and magnetic properties as iron. The alloy ratio of copper and iron can be freely adjusted as needed. The ratio of copper can be from 10% to 90%. 1. Application of copper ferro alloy Copper ferro alloy is mainly used in RF shielding net,connectors,mold and so on. 2. Products of Copper Ferro Alloy Copper ferro alloy rod,copper ferro alloy w...
  • High Quality Cube2pb Tube - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    High Quality Cube2pb Tube - CuCrZr Micro Bore Precision Tube(CuCrZr C15100,C15200,C18150,C18200) – Kinkou

    1. Chemical Composition of CuCrZr Alloy Micro Bore Precision Tube Model Ni Fe Pb Sn Zr Cu C15100 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.15-0.30 Remnant C15200 ≤0.2 ≤0.05 ≤0.01 ≤0.05 0.30-0.50 Remnant Model Cr Fe Pb Si Zr Cu C18150 0.5-1.5 - - - 0.05-0.25 Remnant C18200 0.6-1.2 ≤0.10 ≤0.05 ≤0.01 - Remnant 2. High Precision Indicator(TH04) of CuCrZr Alloy Micro Bore Precision Tube Item External Diameter ...