Hot sale Cw104c Tube - C19160 alloy – Kinkou Detail:
1. Physical properties of C19160
Density | 8.86g/cm3 |
Thermal expansion coefficient | 17.7×10^-6/k |
Thermal conductivity | 210W/(m·K) |
Conductivity | >50%IACS |
Elastic Modulus |
120GPa |
2. Mechanical properties of C19160
State |
size |
Tensile strength |
Yield strength |
Elongation |
Conductivity |
Hardness |
MPa |
MPa |
% |
%ICAS |
HV0.2 |
||
TB00 |
≤40 |
220-360 |
46-72 |
38-45 |
30 |
- |
TH |
≤10 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
10-30 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
|
30-40 |
440-470 |
220-350 |
20-27 |
51-61 |
- |
|
TL |
≤5.0 |
≥620 |
- |
≥5 |
≥50 |
≥165 |
5-6 |
≥590 |
- |
≥5 |
≥50 |
≥165 |
|
6-9.5 |
≥570 |
- |
≥5 |
≥50 |
≥165 |
|
≥9.5 |
≥550 |
- |
≥5 |
≥50 |
≥165 |
3. Application of C19160
C19160 is mainly used in pins, sockets and conductive spring contacts with high strength and elasticity.
Product detail pictures:
Related Product Guide:
The corporate keeps towards the operation concept "scientific administration, superior quality and performance primacy, client supreme for Hot sale Cw104c Tube - C19160 alloy – Kinkou , The product will supply to all over the world, such as: Armenia, Wellington, Turkey, Our aim is to help customers to make more profits and realize their goals. Through a lot of hard work, we establish a long-term business relationship with so many customers all around the world, and achieve win-win success. We will continue to do our best effort to service and satisfy you! Sincerely welcome you to join us!
By Dominic from Bolivia - 2018.08.12 12:27
Company director has very rich management experience and strict attitude, sales staff are warm and cheerful, technical staff are professional and responsible,so we have no worry about product,a nice manufacturer.
By Letitia from Bangalore - 2018.07.26 16:51
Write your message here and send it to us