Short Lead Time for C17200 Rod - C19160 alloy – Kinkou
Short Lead Time for C17200 Rod - C19160 alloy – Kinkou Detail:
1. Physical properties of C19160
Density | 8.86g/cm3 |
Thermal expansion coefficient | 17.7×10^-6/k |
Thermal conductivity | 210W/(m·K) |
Conductivity | >50%IACS |
Elastic Modulus |
120GPa |
2. Mechanical properties of C19160
State |
size |
Tensile strength |
Yield strength |
Elongation |
Conductivity |
Hardness |
MPa |
MPa |
% |
%ICAS |
HV0.2 |
||
TB00 |
≤40 |
220-360 |
46-72 |
38-45 |
30 |
- |
TH |
≤10 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
10-30 |
490-550 |
410-490 |
15-20 |
60-51 |
- |
|
30-40 |
440-470 |
220-350 |
20-27 |
51-61 |
- |
|
TL |
≤5.0 |
≥620 |
- |
≥5 |
≥50 |
≥165 |
5-6 |
≥590 |
- |
≥5 |
≥50 |
≥165 |
|
6-9.5 |
≥570 |
- |
≥5 |
≥50 |
≥165 |
|
≥9.5 |
≥550 |
- |
≥5 |
≥50 |
≥165 |
3. Application of C19160
C19160 is mainly used in pins, sockets and conductive spring contacts with high strength and elasticity.
Product detail pictures:
Related Product Guide:
We retain improving upon and perfecting our items and repair. At the same time, we perform actively to do research and progress for Short Lead Time for C17200 Rod - C19160 alloy – Kinkou , The product will supply to all over the world, such as: Boston, Greece, Hyderabad, We also provide OEM service that caters to your specific needs and requirements. With a strong team of experienced engineers in hose design and development, we value every opportunity to provide best products for our customers.
By Adam from Swaziland - 2017.07.28 15:46
In general, we are satisfied with all aspects, cheap, high-quality, fast delivery and good procuct style, we will have follow-up cooperation!
By Steven from French - 2018.05.13 17:00
Write your message here and send it to us